Corrosion Of Galvanized Potable Water Piping

corrosion pitting in galvanized nipple

I.D. of a galvanized carbon steel nipple from the cold water inlet connection of a residential water heater. Tubercles have formed on the I.D. in low flow conditions. Underneath the tubercles are deep corrosion pits. The cold water chemistry exhibited a Langelier Index of - 0.31 and contained 8 ppm of dissolved oxygen.

 

 

 

 

 

  < < < click here to go back to the previous page  ::

Last Updated: Thursday, February 19, 2004 11:09 AM
Copyright © 2001-2004 The Hendrix Group. All Rights Reserved.

The Hendrix Group, Inc.
15823 N. Barkers Landing
Houston, Texas 77079
Phone: (281) 556-8774
Fax: (281) 870-0659
Email: info@hghouston.com



Technical Reference | Engineering Services | Case Histories | Index
Sitemap | Links | Search | Corporate Info | Staff | Contact
Home | Newsletters | Discussion Forums | Members Only

Site Design by M Media