failure analysis Home | Index | Search | Map
A CORROSION AND MATERIALS TECHNOLOGY SITE
Corrosion, Failure Analysis and Materials Selection are our specialities

 

Index

A B C D E F G H I K L M N O P Q R S T U V W Z

paints
    capital project services
    corrosion links
    corrosion, failure analysis, consulting and inspection services
    failure analysis and corrosion services
    Field metallography services
    laboratory and corrosion testing Serivces
    metallurgical, corrosion engineering and failure analysis services

paper mill
    304 stainless steel white water filter screen corrosion

papers
    corrosion, corrosion control and failure analysis download library

petroleum corrosion
    corrosion and failure analysis technical reference

petroleum failure analysis
    corrosion and failure analysis technical reference

petroleum refining
    petroleum refining processes

photographs
    304 stainless steel white water filter screen corrosion
    316 stainless steel intergranular cracking photograph
    carburization of a HP-40 stainless steel ethylene furnace tube
    case history 002 - galvanized water heater pipe corrosion
    case history 003 - carbon steel torsional fatigue
    case history 004 - fastener rotating bending fatigue
    case history 006 - CO-C02-h30 SSC cracking
    case history 007 - polythionic acid cracking of 310SS
    case history 008 - hydrogen embrittlement of AISI 9310 downhole motor coupling
    case history 009 - quench crack in hex head capscrew
    case history 011 - metal dusting
    case history 012 - gear tooth contact fatigue pitting
    case history 013 - hydrogen embrittlement of a ship's anchor
    case history 014 - Rich/Lean Amine exchanger tube
    case history 015 - Polythionic Acid Stress Corrosion Cracking
    case history 016 - Hydrogen Embrittlement of a Riser Bolt Insert
    case history 017 - High-temperature corrosion failure of a 309SS thermal oxidizer wedge divider
    case history 018 - Failure investigation of a LPG product hose
    case history 019 - Failure of a Tank Scaffold Clip
    case history 020 - Rich/Lean Amine exchanger tube
    caustic cracking of 304 stainless steel photograph
    chloride stress corrosion cracking photograph
    Corroded gas turbine HP 1st stage blade
    corrosion and failure analysis photographs
    corrosion fatigue cracks in AISI 1020 steel in oil and gas downhole service
    corrosion of a Rene 80 nickel alloy gas turbine blade
    creep (stress rupture) voids in a 304SS stainless steel furnace tube
    Creep voids in RA-330 stainless steel photograph
    dezincification corrosion of admiralty brass
    dezincification corrosion of admiralty brass
    ductile iron microstructure
    Explosive decompression blistering of Viton B
    Explosive decompression blistering of Viton B
    fastener hydrogen embrittlement fracture surface
    fatigue and hydrogen embrittlement fracture of AISI 9310 low alloy steel
    fatigue cracking in a pipeline sample
    Fatigue fracture of a compressor connecting rod
    Fretting fatigue striations on an aluminum gasket
    gear tooth fatigue pit
    gear tooth rolling contact fatigue crack
    gear tooth rolling contact fatigue crack
    gear tooth white etching area
    Graphitization of a carbon steel furnace tube
    Graphitization of a carbon steel furnace tube
    Graphitization of a carbon steel furnace tube
    High-temperature hydrogen attack in a boiler tube
    hot corrosion of a gas turbine nickel alloy
    hot corrosion of aluminide coating on a nickel alloy gas turbine blade
    Hydrogen attack corrosion in a boiler tube
    hydrogen embrittlement (HE) corrosion crack at inclusion
    hydrogen embrittlement crack
    hydrogen embrittlement crack in AISI 9623 low alloy steel
    hydrogen embrittlement cracking of 17-4 stainless steel
    hydrogen embrittlement failure of a ship anchor
    hydrogen embrittlement failure of a ship anchor
    hydrogen embrittlement failure of a ship anchor
    metal dusting photograph
    Quench cracking in AISI 4140 low alloy steel fastener
    Rene 80 nickel alloy microstructure
    SEM photograph of hydrogen embrittlement fracture of a fastener

photos
    case history 002 - galvanized water heater pipe corrosion
    case history 003 - carbon steel torsional fatigue
    case history 004 - fastener rotating bending fatigue
    Case history 005 - chloride stress corrosion cracking
    case history 006 - CO-C02-h30 SSC cracking
    case history 007 - polythionic acid cracking of 310SS
    case history 008 - hydrogen embrittlement of AISI 9310 downhole motor coupling
    case history 010 - Explosive Decompression Failure of a Viton B BOP Seal
    case history 011 - metal dusting
    case history 012 - gear tooth contact fatigue pitting
    case history 013 - hydrogen embrittlement of a ship's anchor
    gear tooth fatigue pit
    gear tooth rolling contact fatigue crack
    gear tooth rolling contact fatigue crack
    gear tooth white etching area
    hydrogen embrittlement failure of a ship anchor
    hydrogen embrittlement failure of a ship anchor
    hydrogen embrittlement failure of a ship anchor
    hydrogen embrittlement failure of a ship anchor

pinion
    case history 012 - gear tooth contact fatigue pitting

pinion gear
    gear tooth fatigue pit
    gear tooth rolling contact fatigue crack
    gear tooth rolling contact fatigue crack
    gear tooth white etching area

pipeline
    fatigue cracking in a pipeline sample

pits
    Corrosion of galvanized potable water piping
    gear tooth fatigue pit
    gear tooth rolling contact fatigue crack
    gear tooth rolling contact fatigue crack
    gear tooth white etching area

pitting
    304 stainless steel white water filter screen corrosion
    case history 012 - gear tooth contact fatigue pitting
    cleaning stainless steels
    Corrosion of galvanized potable water piping
    gear tooth fatigue pit
    gear tooth rolling contact fatigue crack
    gear tooth rolling contact fatigue crack
    gear tooth white etching area
    seawater corrosion of stainless steels
    stainless steel categories
    stainless steel corrosion, physical and mechanical property data

platinum aluminide coating
    Corroded gas turbine HP 1st stage blade

polythionic acid
    Polythionic acid stress corrosion cracking of 310 stainless steel

polythionic acid cracking
    case history 007 - polythionic acid cracking of 310SS

potable water
    case history 002 - galvanized water heater pipe corrosion
    Corrosion of galvanized potable water piping

potassium hydroxide
    corrosion - caustic soda service graph
    corrosion - caustic soda service graph
    corrosion and stress corrosion cracking in caustic (caustic soda)
    corrosion resistance of alloys in caustic (sodium hydroxide) solutions

precipitation hardening stainless steel
    hydrogen embrittlement cracking of 17-4 stainless steel

pressure vessel
    pressure vessel guidelines

pressure vessel codes
    pressure vessel guidelines

pressure vessel cracking
    pressure vessel guidelines

pressure vessel failures
    pressure vessel guidelines

pressure vessels
    risk-based inspection and mechanical integrity services

progressive pitting
    case history 012 - gear tooth contact fatigue pitting

publications
    corrosion, corrosion control and failure analysis download library

pyrolysis furnace
    creep (stress rupture) voids in a 304SS stainless steel furnace tube

pyrolysis heater tube
    carburization of a HP-40 stainless steel ethylene furnace tube

Back to Top

  < < < click here to go back to the previous page  ::

Last Updated: Friday, February 20, 2004 11:14 AM
Copyright © 2001-2004 The Hendrix Group. All Rights Reserved.

The Hendrix Group, Inc.
15823 N. Barkers Landing
Houston, Texas 77079
Phone: (281) 556-8774
Fax: (281) 870-0659
Email: hg@hghouston.com



Technical Reference | Engineering Services | Case Histories | Index
Sitemap | Links | Search | Corporate Info | Staff | Contact
Home | Newsletters | Discussion Forums | Members Only

Site Design by M Media