Question:

"Iam looking form corrosion CS Pipes ASTM A106 Gr B Hot flue gases from Gas turbine generator Exhaust temperature ranging from 300 to 400 degree centigrade is used to heat-up Hotoil system which is circuated through the pipe coil inside the exhaust.The flue gases has high Co2 around 50 to 60% and So2. "

Answer:

I would not recommend using A106 carbon steel pipe for your stated application due to the potential for sulfurous acid corrosion at dew point conditions when the unit was shut down.
 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

  < < < click here to go back to the previous page  ::

Last Updated: Monday, March 28, 2005 10:48 AM
Copyright © 2002 The Hendrix Group. All Rights Reserved.

The Hendrix Group, Inc.
15823 N. Barkers Landing
Houston, Texas 77079
Phone: (281) 556-8774
Fax: (281) 870-0659
Email: info@hghouston.com



Technical Reference | Engineering Services | Case Histories | Index
Sitemap | Links | Search | Corporate Info | Staff | Contact
Home | Newsletters | Discussion Forums | Members Only

Site Design by M Media